Alloy K500 is made up of high concentrations of nickel and chromium. The Monel K500 is produced with superior strength and hardness. These alloys are highly resistant to all forms of corrosion and oxidation. They are designed to suffice in high temperatures and extreme pressures. The Monel K500 material possesses superior mechanical properties. They have a minimum tensile strength of 140Ksi and a minimum yield strength of 100Ksi. The alloy is available in hardness of 280 Rockwell and can be easily elongated by 29%. They are widely used in oil and gas refineries, paper production, sensors, electric components chemical industries, etc. We are the leading Monel K500 suppliers. Our goal is to supply the best products in all our outlets which are available at feasible rates.
The Monel Alloy K500 is non-magnetic in low as well as high temperatures. The alloys have exceptional dimensional accuracy and excellent fatigue resistance. They don’t require a lot of maintenance and have a long service life. The Monel K500 Price per kg in India is available in prices between Rs 1200 to Rs 1600. The thickness, size, and other features influence the pricing of the products in this grade. Visit our outlets to get an exact quote on these products as well as our other products.
We are the Alloy K500 suppliers who make use of the latest technology and the best raw materials to produce the best products in the market. These products are produced under the strict guidance of our workers, following all rules and norms set by international and national unions. If you want to get a quote on our products or want to know more about them, contact us for more information.
Standard | Monel K500 |
---|---|
UNS | N05500 |
Werkstoff Nr. | 2.4375 |
Monel K500 Round Bar
Monel K500 Bolts
Monel K500 Rod
Monel K500 Flanges
Monel K500 | |
Ni | 63.0 min |
Fe | 0.5 – 2 |
C | 0.25 max |
Mn | 1.5 max |
Si | 0.5 max |
Cu | 27.0 – 33.0 |
Al | 2.3 – 3.15 |
Ti | 0.35 – 0.85 |
S | 0.010 max |
Density | 8.44 g/cm3 |
Melting Point | 1350 °C (2460 °F) |
Tensile Strength | Psi – 160000 , MPa – 1100 |
Yield Strength (0.2%Offset) | Psi – 115000 , MPa – 790 |
Elongation | 20 % |